Solution:
Concept: In the Hall–Héroult cell the electrolyte is a fused mixture of alumina (about 20%), cryolite, Na₃AlF₆ (about 60%) and fluorspar, CaF₂ (about 20%), kept at about 950 °C. Thick graphite rods dipping into it are the anodes (+), and the carbon lining of the steel tank is the cathode (−).
(i) Other components of the electrolyte and their roles
Step 1 — List the electrolyte.
The fused electrolyte is a mixture of three substances.
| Substance | Formula | Share |
|---|
| Alumina | Al₂O₃ | about 20% |
| Cryolite | Na₃AlF₆ | about 60% |
| Fluorspar | CaF₂ | about 20% |
Step 2 — Give the role of cryolite.
Cryolite dissolves the alumina and lowers the fusion temperature of the mixture from about 2050 °C (pure alumina) to about 950 °C. It also increases the electrical conductivity, since pure alumina is a very poor conductor.
Step 3 — Give the role of fluorspar.
Fluorspar acts, with cryolite, as a solvent for the alumina; it lowers the fusion temperature a little further and increases the conductivity of the melt.
(ii) Why powdered coke is sprinkled on the electrolyte
Step 4 — Explain the coke layer.
A layer of powdered coke on the surface of the bath does two jobs. It reduces the loss of heat by radiation from the hot surface, and it prevents the hot graphite anodes from burning in the air at the surface.

Watch out: Cryolite and fluorspar are added to the ELECTROLYTE; coke is only sprinkled on top of it.
Therefore, (i) cryolite (lowers the fusion temperature and increases conductivity) and fluorspar (solvent that increases conductivity); (ii) powdered coke reduces heat loss by radiation and prevents the anodes burning in air.