Write the constituents of electrolyte for the extraction of aluminium
Metallurgy · Question 80 of 85
Write the constituents of electrolyte for the extraction of aluminium
Solution:
Concept: The electrolyte is a molten mixture of alumina, cryolite and fluorspar in the ratio 1 : 3 : 1, kept at about 950 °C.
Step 1 — List the constituents.
The table gives each constituent and its share.
| Constituent | Formula | Share |
|---|---|---|
| Alumina | 20% | |
| Cryolite | 60% | |
| Fluorspar | 20% |
Step 2 — Check the ratio.
The shares 20 : 60 : 20 simplify (dividing by 20) to 1 : 3 : 1, and they add up to 100%.
Step 3 — Note the coke layer.
Powdered coke is sprinkled on the surface of the electrolyte to reduce heat loss and to stop the anodes burning in air.

Watch out: Pure alumina alone would need about 2050 °C; cryolite and fluorspar bring the working temperature down to about 950 °C.
Therefore, the electrolyte is fused alumina (20%), cryolite (60%) and fluorspar (20%).