Cognitive domain: Analysis A handicraft workshop in Moradabad nickel-plates small brass key rings.

Question 384 marksHard

Cognitive domain: Analysis

A handicraft workshop in Moradabad nickel-plates small brass key rings. The cleaned rings hang from the rack that serves as the cathode, in a bath of nickel sulphate solution acidified with a little dilute sulphuric acid. The anode is a plate of pure nickel, and a steady, low direct current is passed. The supervisor weighs the rack with its rings at intervals. (Hypothetical data.)

Time (minutes)020406090
Mass of rack with rings (g)120.00120.40120.80121.20121.80

(a) Find the gain in mass in every 20 minutes, and predict the mass of the rack with its rings after 120 minutes.

(b) Write the reaction at each electrode during normal plating. On another day a fresh batch of rings, again 120.00 g with the rack, is plated with the same current. After 40 minutes the leads are swapped by mistake, so for the next 20 minutes the rack is joined to the positive terminal. Assume that the nickel coat covers each ring completely. Predict the mass of the rack with its rings at 60 minutes, and explain what happens at each electrode during those 20 minutes.

(c) To save money, the supervisor wants to use a lump of scrap nickel containing iron and copper as the anode. Using the electrochemical series, say what would happen to each impurity, and give your advice.