The rise in temperature is a measure of how vigorously each metal reacts with the acid, because the reactions of metals with dilute acids give out heat. A bigger rise means a faster reaction.
(a) At ordinary temperature the surfaces of metals such as magnesium, aluminium and zinc are covered with a thin layer of oxide, and on aluminium this layer is especially protective. When an unrubbed piece of aluminium is put into the acid, the acid first has to remove the oxide layer before it can reach the metal. Until then hardly any hydrogen is given off, so the reaction starts slowly and only a small rise in temperature (3 °C) is recorded in 5 minutes.
The low reading is therefore caused by the oxide layer, not by aluminium being less reactive than zinc. The book tells us to rub tarnished samples clean with sandpaper first. With clean samples, aluminium reacts faster than zinc, and the order is
Mg>Al>Zn>Fe
for example:
2Al(s)+6HCl(aq)→2AlCl3(aq)+3H2(g)
(b) The temperature rise for copper is 0 °C: no bubbles and no change in temperature, so copper does not react with dilute hydrochloric acid. Copper lies below hydrogen in the reactivity series, so it cannot displace hydrogen from the acid. (Magnesium, aluminium, zinc and iron all lie above hydrogen, which is why each of them does react.)

The reactivity series: what each metal reacts with, and how it is obtained from its ore.