Confirming your payment

Skip to content

Sign up now and get .

Opening your dashboard

Class 12 Chemistry Chapter 6 General Principles and Processes of Isolation of Elements: Previous Year Questions

8 questions on Chapter 6, each solved step by step. Class 12 Chemistry, ICSE 2026-27.

8 questions with solutions

1–3 marks · Mixed difficulty

  1. 1

    Question 1

    Name the important ore of silver. Write all the steps and reactions involved in the Cyanide process for the extraction of silver from its ore.

    MediumAsked 2015
    3 marks
    Solve with AI
    Written solution

    Solution:

    Key idea: In the cyanide process (a hydrometallurgical method), silver is first dissolved out of its ore as a soluble cyanide complex (leaching) and then displaced from the solution by a more electropositive metal, zinc.

    Step 1 — Name the important ore of silver.

    The important ore of silver is argentite (silver glance), Ag2S\mathrm{Ag_2S}. Silver also occurs as horn silver (AgCl\mathrm{AgCl}) and in the native (free) state.

    Step 2 — Concentrate the ore.

    The sulphide ore is crushed, powdered and concentrated by the froth flotation process, which separates the sulphide particles from the earthy gangue.

    Step 3 — Leach the ore with sodium cyanide.

    The concentrated ore is treated with a dilute (about 0.5 %) solution of sodium cyanide while air is blown through it. Silver sulphide dissolves as the soluble complex sodium dicyanoargentate(I).

    Ag2S+4NaCN⇌2Na[Ag(CN)2]+Na2S\mathrm{Ag_2S + 4NaCN \rightleftharpoons 2Na[Ag(CN)_2] + Na_2S}

    This reaction is reversible. Oxygen of the air oxidises the sodium sulphide formed to sodium sulphate, which removes Na2S\mathrm{Na_2S} from the mixture and drives the reaction forward.

    Na2S+2O2⟶Na2SO4\mathrm{Na_2S + 2O_2 \longrightarrow Na_2SO_4}

    Step 4 — Precipitate silver with zinc.

    The solution of Na[Ag(CN)2]\mathrm{Na[Ag(CN)_2]} is filtered and zinc dust is added. Zinc is more electropositive than silver, so it displaces silver from the complex, and silver separates as a black precipitate.

    2Na[Ag(CN)2]+Zn⟶Na2[Zn(CN)4]+2Ag\mathrm{2Na[Ag(CN)_2] + Zn \longrightarrow Na_2[Zn(CN)_4] + 2Ag}

    Step 5 — Recover and refine the silver.

    The precipitate is filtered off and fused with a little potassium nitrate, which oxidises the excess zinc so that it can be removed, and the molten silver is cast. The silver obtained is refined electrolytically. Impure silver is made the anode, a thin sheet of pure silver is the cathode, and a solution of silver nitrate acidified with a little nitric acid is the electrolyte. On passing current, silver dissolves from the anode as Ag+\mathrm{Ag^+} ions and pure silver is deposited on the cathode.

    Anode: Ag⟶Ag++e−\mathrm{Anode:\ Ag \longrightarrow Ag^+ + e^-} Cathode: Ag++e−⟶Ag\mathrm{Cathode:\ Ag^+ + e^- \longrightarrow Ag}

    Note: Sodium cyanide is extremely poisonous. Cyanide solutions are kept alkaline (with lime) so that poisonous hydrogen cyanide gas is not given off, and the spent solutions are treated to destroy the cyanide before they are released.

    Therefore, the ore is argentite (Ag₂S); in the cyanide process it is concentrated by froth flotation, leached with NaCN in air to form Na[Ag(CN)₂] (Na₂S being oxidised to Na₂SO₄), silver is precipitated from the complex by zinc, and the crude silver is refined electrolytically.

  2. 2

    Question 2

    Give the balanced equations for the conversion of argentite (Ag2S\mathrm{Ag_2S}) to metallic silver.

    MediumAsked 2017
    2 marks
    Solve with AI
    Written solution

    Solution:

    Key idea: Argentite is changed to silver by the cyanide process: the ore is leached with sodium cyanide in the presence of air, and silver is then displaced from the soluble cyanide complex by zinc.

    Step 1 — Dissolve argentite in sodium cyanide.

    Argentite reacts with a dilute solution of sodium cyanide to form the soluble complex sodium dicyanoargentate(I).

    Ag2S+4NaCN⇌2Na[Ag(CN)2]+Na2S\mathrm{Ag_2S + 4NaCN \rightleftharpoons 2Na[Ag(CN)_2] + Na_2S}

    Step 2 — Drive the reaction forward with air.

    The first reaction is reversible. Air blown through the mixture oxidises the sodium sulphide to sodium sulphate, removing it and pushing the first reaction to completion.

    Na2S+2O2⟶Na2SO4\mathrm{Na_2S + 2O_2 \longrightarrow Na_2SO_4}

    Step 3 — Displace silver with zinc.

    Zinc dust added to the filtered solution displaces metallic silver, because zinc is more electropositive than silver.

    2Na[Ag(CN)2]+Zn⟶Na2[Zn(CN)4]+2Ag\mathrm{2Na[Ag(CN)_2] + Zn \longrightarrow Na_2[Zn(CN)_4] + 2Ag}

    Note: Sodium cyanide is extremely poisonous. Cyanide solutions are kept alkaline (with lime) so that poisonous hydrogen cyanide gas is not given off, and the spent solutions are treated to destroy the cyanide before they are released.

    Therefore, the balanced equations are Ag₂S + 4NaCN ⇌ 2Na[Ag(CN)₂] + Na₂S, Na₂S + 2O₂ → Na₂SO₄ and 2Na[Ag(CN)₂] + Zn → Na₂[Zn(CN)₄] + 2Ag.

  3. 3

    Question 3

    Complete the following statements by selecting the correct alternative from the choices given:

    Purification of aluminium by electrolytic refining is called:

    MCQEasyAsked 2018
    1 mark
    Solve with AI
    Answer
    • (A) Serpeck's process

    • (B) Hoope's process

      Correct
    • (C) Hall's process

    • (D) Baeyer's process

    Answer: (B) Hoope's process

    Key idea: Hoope's process refines impure aluminium electrolytically in a cell with three molten layers of different densities.

    Step 1 — Describe the three layers.

    The bottom layer is the anode: impure aluminium alloyed with copper, which makes it heavy. The middle layer is the electrolyte: fused fluorides of aluminium, sodium and barium (cryolite with barium fluoride). The top layer is pure molten aluminium, which acts as the cathode through graphite rods dipping into it.

    Step 2 — Explain how the metal is purified.

    When current passes, aluminium from the bottom layer goes into the electrolyte as Al3+\mathrm{Al^{3+}} ions, and these are discharged at the top layer as pure aluminium. Impurities such as copper and silicon stay behind in the bottom layer, so aluminium of about 99.98 % purity collects at the top.

    Why the others are wrong:

    • (A) Serpeck's process purifies bauxite that contains silica as the main impurity: the bauxite is heated with coke in nitrogen to form aluminium nitride, which water then hydrolyses to aluminium hydroxide.
    • (C) Hall's process purifies bauxite by fusing it with sodium carbonate; the related electrolysis of alumina in fused cryolite (the Hall–Héroult process) extracts aluminium but does not refine it.
    • (D) Baeyer's process purifies bauxite (with iron oxide as the main impurity) by digesting it with sodium hydroxide solution.

    Therefore, the electrolytic refining of aluminium is Hoope's process, option (B).

  4. 4

    Question 4

    Name the sulphide ore of Copper. Describe how pure copper is extracted from this ore.

    MediumAsked 2018
    3 marks
    Solve with AI
    Written solution

    Solution:

    Key idea: Copper is extracted from its sulphide ore by concentration, roasting, smelting to a matte, and self-reduction of the sulphide in a Bessemer converter; the crude (blister) copper is finally refined electrolytically.

    Step 1 — Name the sulphide ore.

    The chief sulphide ore of copper is copper pyrites (chalcopyrite), CuFeS2\mathrm{CuFeS_2}. Copper glance, Cu2S\mathrm{Cu_2S}, is another sulphide ore.

    Step 2 — Concentrate the ore.

    The crushed ore is concentrated by the froth flotation process, which collects the sulphide particles in the froth and leaves the gangue behind.

    Step 3 — Roast the concentrate.

    The concentrate is heated in a current of air in a reverberatory furnace. Moisture and volatile impurities are removed (sulphur as SO2\mathrm{SO_2}, arsenic as As2O3\mathrm{As_2O_3}), and copper pyrites is partly changed into the sulphides of copper and iron.

    2CuFeS2+O2⟶Cu2S+2FeS+SO2\mathrm{2CuFeS_2 + O_2 \longrightarrow Cu_2S + 2FeS + SO_2}

    Step 4 — Smelt the roasted ore to a matte.

    The roasted ore is mixed with silica and a little coke and heated strongly in a blast furnace. Iron sulphide is oxidised to ferrous oxide, which combines with silica to form a slag of ferrous silicate that floats on top and is removed.

    2FeS+3O2⟶2FeO+2SO2\mathrm{2FeS + 3O_2 \longrightarrow 2FeO + 2SO_2} FeO+SiO2⟶FeSiO3\mathrm{FeO + SiO_2 \longrightarrow FeSiO_3}

    Any cuprous oxide formed is changed back to cuprous sulphide by iron sulphide, so copper is not lost in the slag.

    Cu2O+FeS⟶Cu2S+FeO\mathrm{Cu_2O + FeS \longrightarrow Cu_2S + FeO}

    The molten mixture left, mainly Cu2S\mathrm{Cu_2S} with a little FeS, is called copper matte.

    Step 5 — Convert the matte to blister copper.

    The molten matte is put into a Bessemer converter with a little silica, and a blast of air is blown through it. The remaining FeS is removed as slag in the same way, and part of the cuprous sulphide is oxidised to cuprous oxide.

    2Cu2S+3O2⟶2Cu2O+2SO2\mathrm{2Cu_2S + 3O_2 \longrightarrow 2Cu_2O + 2SO_2}

    The cuprous oxide then reacts with the unchanged cuprous sulphide, giving copper metal (self-reduction).

    2Cu2O+Cu2S⟶6Cu+SO2\mathrm{2Cu_2O + Cu_2S \longrightarrow 6Cu + SO_2}

    The copper obtained is about 98 % pure. As it solidifies, dissolved SO2\mathrm{SO_2} escapes and leaves blisters on its surface, so it is called blister copper.

    Step 6 — Refine the blister copper.

    Blister copper is first refined by poling and then by electrolysis. Impure copper is made the anode, a thin sheet of pure copper the cathode, and copper sulphate solution acidified with sulphuric acid the electrolyte. Copper dissolves at the anode and pure copper is deposited on the cathode; less reactive metals such as silver and gold collect below the anode as anode mud.

    Anode: Cu⟶Cu2++2e−\mathrm{Anode:\ Cu \longrightarrow Cu^{2+} + 2e^-} Cathode: Cu2++2e−⟶Cu\mathrm{Cathode:\ Cu^{2+} + 2e^- \longrightarrow Cu}

    Note: Sulphur dioxide is a poisonous, choking gas that also causes acid rain, so smelters collect it and convert it into sulphuric acid instead of releasing it.

    Therefore, the sulphide ore is copper pyrites (CuFeS₂); pure copper is obtained by froth flotation, roasting, smelting with silica to a matte, self-reduction of Cu₂S in a Bessemer converter to blister copper, and electrolytic refining.

  5. 5

    Question 5

    Fill in the blanks by choosing the appropriate words from those given in the brackets.

    (More than, primary, cathode, Lucas, regent, two, four, less than, Grignard's reagent, tertiary, anode, zero, equal to, three)

    In electrolytic refining the impure metal is made ______ While a thin sheet of pure metal is used as ______

    EasyAsked 2019
    1 mark
    Solve with AI
    Written solution

    Solution:

    Key idea: In electrolytic refining, metal dissolves from the anode as ions and the same ions are discharged as pure metal at the cathode.

    Step 1 — Place the impure metal.

    The impure metal must lose metal atoms as ions into the electrolyte, and oxidation (loss of electrons) happens at the anode. So the impure metal is made the anode.

    Step 2 — Place the pure metal sheet.

    The metal ions are reduced and deposited at the cathode. A thin sheet of the pure metal is used as the cathode, and pure metal builds up on it, while the impurities either stay in solution or fall as anode mud.

    Therefore, in electrolytic refining the impure metal is made the anode, while a thin sheet of pure metal is used as the cathode.

  6. 6

    Question 6

    Describe the role of the following.

    I) Cryolite in the extraction of aluminum from pure alumina.

    II) NaCN in the extraction of silver from a silver ore.

    III) Coke in the extraction of iron from its oxides.

    MediumAsked 2019
    3 marks
    Solve with AI
    Written solution

    Solution:

    Key idea: Each named substance makes its extraction possible or practical: cryolite lowers the melting point of the electrolyte, sodium cyanide dissolves silver as a complex, and coke supplies both heat and the reducing agent.

    Step 1 — (I) Explain the role of cryolite.

    Pure alumina melts only above 2300 K (about 2050 °C), and molten alumina conducts electricity poorly. Alumina is therefore dissolved in molten cryolite, Na3AlF6\mathrm{Na_3AlF_6} (with a little CaF2\mathrm{CaF_2}). This mixture melts and can be electrolysed at about 1173–1273 K, and it conducts electricity well. Cryolite thus lowers the working temperature, which saves a great deal of energy, and increases the conductivity of the melt.

    Step 2 — (II) Explain the role of NaCN.

    Sodium cyanide is the leaching agent in the cyanide process. It dissolves silver out of the ore as the soluble complex sodium dicyanoargentate(I), leaving the gangue behind.

    Ag2S+4NaCN⇌2Na[Ag(CN)2]+Na2S\mathrm{Ag_2S + 4NaCN \rightleftharpoons 2Na[Ag(CN)_2] + Na_2S}

    Silver is later displaced from this solution by zinc.

    Step 3 — (III) Explain the role of coke as a fuel.

    In the blast furnace, coke burns in the hot air blast near the bottom. The reaction gives out a large amount of heat, which keeps the furnace at the high temperature needed.

    C+O2⟶CO2\mathrm{C + O_2 \longrightarrow CO_2}

    Step 4 — (III) Explain the role of coke as the reducing agent.

    Higher up, the carbon dioxide reacts with more coke to give carbon monoxide, which is the main reducing agent for the iron oxide.

    CO2+C⟶2CO\mathrm{CO_2 + C \longrightarrow 2CO} Fe2O3+3CO⟶2Fe+3CO2\mathrm{Fe_2O_3 + 3CO \longrightarrow 2Fe + 3CO_2}

    In the hotter lower part, coke also reduces ferrous oxide directly.

    FeO+C⟶Fe+CO\mathrm{FeO + C \longrightarrow Fe + CO}

    Note: Sodium cyanide is extremely poisonous, so its solutions are kept alkaline (no hydrogen cyanide gas) and treated before release. Carbon monoxide is also poisonous; the blast-furnace gas is collected and burnt as a fuel.

    Therefore, (I) cryolite lowers the melting point of alumina and increases the conductivity of the melt; (II) NaCN dissolves silver from its ore as the soluble complex Na[Ag(CN)₂]; (III) coke is the fuel that heats the blast furnace and the source of CO (and C) that reduces iron oxide to iron.

  7. 7

    Question 7

    Fill in the blanks by choosing the appropriate word/words from those given in the brackets:

    (iodoform, volume, mass, haloform, gram equivalent, chloroform, carbylamine, sp3d2\mathrm{sp^3d^2}, high, coke, d2sp3\mathrm{d^2sp^3}, low, gram mole, carbon monoxide)

    Zinc oxide is reduced by ______ at 1673K to form zinc and ______.

    EasyAsked 2020
    1 mark
    Solve with AI
    Written solution

    Solution:

    Key idea: Zinc oxide is reduced by carbon (coke) at a high temperature; above about 1000 K carbon is oxidised mainly to carbon monoxide rather than carbon dioxide.

    Step 1 — Write the reduction.

    Zinc oxide is heated with coke at 1673 K. Carbon takes the oxygen from zinc oxide and forms carbon monoxide.

    ZnO+C→1673 KZn+CO\mathrm{ZnO + C \xrightarrow{1673\ K} Zn + CO}

    Step 2 — Note how the zinc is collected.

    Zinc boils at about 1180 K, so at 1673 K it comes off as vapour and is condensed separately.

    Note: Carbon monoxide is a poisonous gas, so the zinc furnace gases are collected and burnt rather than released.

    Therefore, zinc oxide is reduced by coke at 1673 K to form zinc and carbon monoxide.

  8. 8

    Question 8

    Name an important ore of silver. How is silver extracted from its sulphide ore? Give balanced chemical equations involved in the extraction of pure silver.

    MediumAsked 2020
    3 marks
    Solve with AI
    Written solution

    Solution:

    Key idea: Silver is extracted from its sulphide ore by the cyanide process: the ore is leached with sodium cyanide in air, silver is displaced from the cyanide complex by zinc, and the crude silver is refined electrolytically.

    Step 1 — Name an important ore of silver.

    The important ore of silver is argentite (silver glance), Ag2S\mathrm{Ag_2S}. Silver also occurs as horn silver (AgCl\mathrm{AgCl}) and in the native (free) state.

    Step 2 — Concentrate the ore.

    The powdered sulphide ore is concentrated by the froth flotation process.

    Step 3 — Leach the ore with sodium cyanide.

    The concentrated ore is treated with a dilute (about 0.5 %) solution of sodium cyanide while air is blown through it. Silver sulphide dissolves as the soluble complex sodium dicyanoargentate(I).

    Ag2S+4NaCN⇌2Na[Ag(CN)2]+Na2S\mathrm{Ag_2S + 4NaCN \rightleftharpoons 2Na[Ag(CN)_2] + Na_2S}

    This reaction is reversible. Oxygen of the air oxidises the sodium sulphide formed to sodium sulphate, which removes Na2S\mathrm{Na_2S} from the mixture and drives the reaction forward.

    Na2S+2O2⟶Na2SO4\mathrm{Na_2S + 2O_2 \longrightarrow Na_2SO_4}

    Step 4 — Precipitate silver with zinc.

    The solution of Na[Ag(CN)2]\mathrm{Na[Ag(CN)_2]} is filtered and zinc dust is added. Zinc is more electropositive than silver, so it displaces silver from the complex, and silver separates as a black precipitate.

    2Na[Ag(CN)2]+Zn⟶Na2[Zn(CN)4]+2Ag\mathrm{2Na[Ag(CN)_2] + Zn \longrightarrow Na_2[Zn(CN)_4] + 2Ag}

    Step 5 — Refine the crude silver.

    The precipitate is filtered off and fused with a little potassium nitrate, which removes the excess zinc. The silver obtained is refined electrolytically. Impure silver is made the anode, a thin sheet of pure silver is the cathode, and a solution of silver nitrate acidified with a little nitric acid is the electrolyte. On passing current, silver dissolves from the anode as Ag+\mathrm{Ag^+} ions and pure silver is deposited on the cathode.

    Anode: Ag⟶Ag++e−\mathrm{Anode:\ Ag \longrightarrow Ag^+ + e^-} Cathode: Ag++e−⟶Ag\mathrm{Cathode:\ Ag^+ + e^- \longrightarrow Ag}

    Note: Sodium cyanide is extremely poisonous. Cyanide solutions are kept alkaline (with lime) so that poisonous hydrogen cyanide gas is not given off, and the spent solutions are treated to destroy the cyanide before they are released.

    Therefore, the ore is argentite (Ag₂S); silver is extracted by leaching with NaCN in air (Ag₂S + 4NaCN ⇌ 2Na[Ag(CN)₂] + Na₂S, Na₂S + 2O₂ → Na₂SO₄), precipitation with zinc (2Na[Ag(CN)₂] + Zn → Na₂[Zn(CN)₄] + 2Ag) and electrolytic refining.