Which process is generally used for the concentration of sulphide ores?
General Principles and Processes of Isolation of Elements · Question 106 of 228
Which process is generally used for the concentration of sulphide ores?
Solution:
Key idea: Froth flotation separates particles by the way their surfaces are wetted. Sulphide mineral particles are wetted mainly by oil, while the gangue (sand and rock) is wetted by water.
Step 1 — Prepare the ore mixture.
The finely powdered ore is mixed with water in a tank. A collector such as pine oil or a xanthate is added, which coats the sulphide particles and makes them water-repelling, and a froth stabiliser such as cresol or aniline is added to keep the froth from collapsing.
Step 2 — Blow air through to make a froth.
Air is blown in and the mixture is stirred, which makes a froth of bubbles. The oil-coated sulphide particles stick to the air bubbles and rise into the froth, which is skimmed off and dried to give the concentrated ore. The gangue particles, wetted by water, settle at the bottom.
Watch out: Flotation does not work by density. Sulphide minerals (for example PbS, about 7.6 g cm⁻³) are denser than the gangue (quartz, about 2.65 g cm⁻³), yet they rise because they cling to the air bubbles.
Therefore, sulphide ores are generally concentrated by the froth flotation process.