(a) Name the purest form of iron
(b) Name the reducing agents which reduce FeO to Fe above 1073 K and below 1073 K.
(c) Write the formula of slags formed during the extraction of Fe from ore and during the extraction of Cu from ore.
Confirming your payment
Sign up now and get 250 free tokens.
General Principles and Processes of Isolation of Elements · Question 200 of 228
(a) Name the purest form of iron
(b) Name the reducing agents which reduce FeO to Fe above 1073 K and below 1073 K.
(c) Write the formula of slags formed during the extraction of Fe from ore and during the extraction of Cu from ore.
Solution:
Key idea: The commercial forms of iron differ in how much carbon they hold. In the blast furnace both carbon and carbon monoxide reduce FeO, each over its own temperature range. A flux combines with the gangue to give an easily fusible slag.
Step 1 — Name the purest form of iron (part a).
Wrought iron is the purest commercial form of iron, because puddling oxidises away almost all the carbon and the other impurities of cast iron. It contains very little carbon, below about 0.1 %.
Note: Older textbooks quote 0.12–0.25 % carbon for wrought iron; that range overlaps mild steel, and real wrought iron holds less than about 0.1 %.
Step 2 — Name the reducing agents for FeO (part b).
Above about 1073 K the C–CO line of the Ellingham diagram lies below the Fe–FeO line, so coke (carbon) itself reduces FeO.
Below about 1073 K carbon cannot do this, and the reduction is done by carbon monoxide.
Step 3 — Write the slags (part c).
In the extraction of iron the gangue is mainly silica, and limestone is the flux; the lime formed from it combines with the silica.
In the extraction of copper the impurity is iron, present as FeO after roasting, and silica is the flux.
Therefore, (a) the purest form is wrought iron; (b) FeO is reduced by coke (carbon) above 1073 K and by carbon monoxide below 1073 K; (c) the slags are (iron) and (copper).