How do we separate two sulphide ores by Froth Flotation Method? Explain with an example.
General Principles and Processes of Isolation of Elements · Question 155 of 228
How do we separate two sulphide ores by Froth Flotation Method? Explain with an example.
Solution:
Key idea: In froth flotation, sulphide particles made water-repellent by an oil cling to air bubbles and rise in the froth. Two sulphide ores are separated by adding a depressant, which stops one of them from joining the froth.
Step 1 — Recall how a single sulphide ore is floated.
The powdered ore is mixed with water, a collector (such as pine oil or a xanthate) and a froth stabiliser, and air is blown through. The collector makes the sulphide particles water-repellent, so they stick to the air bubbles and rise into the froth, while the gangue is wetted by water and stays in the liquid.
Step 2 — Add a depressant to the mixed ore.
Galena (PbS) mixed with zinc blende (ZnS) is a common example. Sodium cyanide is added as a depressant. It reacts with the surface of the ZnS particles and covers them with a layer of the complex sodium tetracyanozincate(II).
Step 3 — Collect the two sulphides one after the other.
The coated ZnS particles are no longer made water-repellent by the oil, so they do not stick to the bubbles and stay in the water. Only PbS comes up with the froth and is skimmed off. The ZnS left behind can then be floated in a second stage after its surface is activated (for example with copper sulphate). Adjusting the proportion of oil to water also helps the separation.
Note: Sodium cyanide is highly toxic; it is used in alkaline slurries so that poisonous HCN gas cannot form.
Therefore, two sulphide ores are separated by froth flotation with a depressant: for PbS mixed with ZnS, NaCN depresses ZnS so that only PbS comes up in the froth.