How is the ore concentrated by froth flotation process? What is the role of stabilizer and of a depressant? Give one example of each.
General Principles and Processes of Isolation of Elements · Question 224 of 228
How is the ore concentrated by froth flotation process?
Solution:
Key idea: In froth flotation the surface of sulphide ore particles is preferentially wetted by oil (a collector), while the gangue is wetted by water. Air bubbles then carry the oil-coated ore particles up into a froth.
Step 1 — Prepare the pulp.
The ore is crushed to a fine powder and mixed with water in a large tank. A small amount of collector (pine oil, fatty acids or potassium ethyl xanthate) and a froth stabiliser are added.
Step 2 — Float the ore particles in the froth.
The mixture is agitated strongly while air is blown through it. The oil-coated ore particles are not wetted by water, so they stick to the air bubbles and are carried up to the surface in the froth. The froth is skimmed off, allowed to collapse and dried. The gangue particles, wetted by water, settle at the bottom. The method is used for sulphide ores such as zinc blende, galena and copper pyrites.
Step 3 — Explain the role of the froth stabiliser.
A froth stabiliser makes the froth last longer, so that the ore particles held in it can be skimmed off before the bubbles burst. Examples are cresols and aniline.
Step 4 — Explain the role of the depressant.
A depressant prevents one sulphide from coming into the froth, so that two sulphide ores can be separated. For example, sodium cyanide keeps ZnS back and lets PbS float from a mixture of the two, by forming a complex on the ZnS surface.
Watch out: The ore particles do not float because the oil makes them lighter. They float because the oil makes their surface water-repellent, so they cling to the air bubbles, which carry them up.
Note: Sodium cyanide is extremely poisonous. Cyanide solutions are kept alkaline (with lime) so that poisonous hydrogen cyanide gas is not given off, and the spent solutions are treated to destroy the cyanide before they are released.
Therefore, in froth flotation the powdered sulphide ore is agitated with water, a collector and air so that the oil-coated ore particles rise with the froth; a froth stabiliser (e.g. cresol) makes the froth last, and a depressant (e.g. NaCN) keeps one sulphide (ZnS) out of the froth.