How is cast iron (or pig. iron) extracted from haematite?
General Principles and Processes of Isolation of Elements · Question 205 of 228
How is cast iron (or pig. iron) extracted from haematite?
Solution:
Key idea: Haematite () is concentrated, roasted and then reduced in a blast furnace, mainly by carbon monoxide made from coke. Limestone is added as a flux so that the silica of the gangue leaves as a fusible slag.
Step 1 — Concentrate the ore.
The ore is crushed and concentrated by gravity separation, because haematite is much denser than the earthy and siliceous gangue, which a stream of water washes away. A magnetic ore such as magnetite can instead be concentrated by magnetic separation.
Step 2 — Roast (calcine) the concentrate.
The concentrated ore is heated in excess of air. This removes moisture and carbon dioxide, oxidises sulphur and arsenic to volatile oxides, and makes the ore porous. Any ferrous oxide is changed to ferric oxide, so that it is not lost later as ferrous silicate slag.
Step 3 — Charge the blast furnace.
The roasted ore is mixed with coke (fuel and reducing agent) and limestone (flux) and fed in at the top of a tall steel furnace lined with fire-bricks. A blast of hot air is blown in near the bottom through pipes called tuyeres, so the furnace is hottest at the bottom and cooler towards the top.
Step 4 — Burn the coke in the lower zone (zone of combustion).
Near the tuyeres, at about 1500–2000 K, coke burns in the hot air and supplies the heat. The carbon dioxide formed rises, meets more hot coke and is reduced to carbon monoxide, the main reducing agent.
Step 5 — Remove the gangue in the middle zone (zone of heat absorption).
In the middle part of the furnace, at about 800–1000 °C, limestone decomposes, and the lime combines with the silica of the gangue to form a fusible slag.
Step 6 — Reduce the oxide in the upper zone (zone of reduction).
In the cooler upper part, at about 500–900 K, the rising carbon monoxide reduces the iron oxides step by step, giving solid spongy iron and some ferrous oxide.
Lower down, in the hotter part, the ferrous oxide is reduced to iron by carbon monoxide and by coke.
Adding up the steps, the overall reduction of haematite by carbon monoxide is written as below.
Step 7 — Melt the iron and let it take up impurities.
The spongy iron moves down, melts in the hot lower zone and dissolves some carbon. Silicon, manganese and phosphorus, formed by the reduction of their oxides by coke, also dissolve in it, for example:
Step 8 — Tap the iron and the slag.
Molten iron collects at the bottom (the hearth). The lighter molten slag floats on it, protects it from oxidation, and is run off through the slag hole. The iron is run out into moulds; this iron is pig iron, which contains about 4 % carbon.
Step 9 — Turn pig iron into cast iron.
Pig iron is remelted with scrap iron and coke in a hot-air blast in a cupola furnace and poured into moulds. The product is cast iron: it contains slightly less carbon than pig iron (about 3 %) and is hard and brittle.
Note: Carbon monoxide is a poisonous gas. The gas leaving the top of the furnace is collected and burnt as a fuel (for example, to preheat the air blast) instead of being released.
Therefore, pig iron is extracted from haematite by concentration, roasting and reduction in a blast furnace with coke and limestone (mainly by carbon monoxide), and cast iron is made by remelting pig iron with scrap iron and coke in a cupola.