Out of Zn and Sn which one protects iron better after crack and why?
Electrochemistry · Question 145 of 241
Out of Zn and Sn which one protects iron better after crack and why?
Solution:
Key idea: When two metals touch in moist air, they form a small galvanic cell. The more electropositive metal (the one with the more negative standard reduction potential) becomes the anode and corrodes, while the other becomes the cathode and is protected. The standard reduction potentials are: −0.76 V, −0.44 V and −0.14 V.
Step 1 — Compare zinc with iron.
Zinc is more electropositive than iron, because its potential (−0.76 V) is more negative than that of iron (−0.44 V). At a crack in a zinc coating, zinc acts as the anode and is oxidised in preference to iron, . The exposed iron acts as the cathode, so it does not rust. This is called sacrificial protection.
Step 2 — Compare tin with iron.
Tin is less electropositive than iron, because its potential (−0.14 V) is less negative than that of iron. At a crack in a tin coating, iron becomes the anode and is oxidised, , while the tin acts as the cathode. So the exposed iron rusts even faster than bare iron.
Step 3 — Decide which coating protects better.
Only zinc goes on protecting iron after the coating is broken, so zinc is the better choice.
Therefore, zinc protects iron better after a crack, because zinc is more electropositive than iron and corrodes in its place, whereas tin makes the exposed iron the anode.