(a)
| Method | Type |
|---|
| Painting | Barrier method: physically isolates the metal from moisture and O2 |
| Galvanising (zinc coating) | Both barrier and electrochemical protection |
| Cathodic protection (external current) | Electrochemical protection method |
| Magnesium block (sacrificial anode) | Electrochemical protection method |
(b) Magnesium has a much lower standard reduction potential (E∘=−2.36 V) than iron (−0.44 V). When a magnesium block is wired to the pipeline, the moist soil acts as the electrolyte and a galvanic cell is formed. Magnesium, the more active metal, becomes the anode and is oxidised in preference to iron:
Mg(s)→Mg2+(aq)+2e−
The electrons flow into the pipeline, which becomes the cathode. There, dissolved oxygen is reduced instead of iron being oxidised. The magnesium is slowly used up in place of the iron, so it is called a sacrificial anode and must be replaced from time to time.
Copper (E∘=+0.34 V) lies above iron. Joined to copper, the iron would become the anode, and the pipeline would corrode faster, not slower.
(c) Slower. At the scratch, zinc and iron are in contact with moisture and form a small galvanic cell. Zinc (−0.76 V) is easier to oxidise than iron (−0.44 V), so the surrounding zinc becomes the anode:
Zn(s)→Zn2+(aq)+2e−
The exposed iron becomes the cathode, where oxygen is reduced, and so it is not oxidised. The zinc keeps protecting the iron electrochemically even after the coating is broken. A scratched painted pipe has no such protection: bare iron at the scratch simply rusts.